PJ-OQ Iyẹwu Meji Igbale epo quenching ileru
Akọkọ sipesifikesonu
koodu awoṣe | Iwọn agbegbe iṣẹ mm | Fifuye agbara kg | Agbara alapapo kw | |||
ipari | igboro | iga | ||||
PJ-OQ | 644 | 600 | 400 | 400 | 200 | 80 |
PJ-OQ | 755 | 700 | 500 | 500 | 300 | 120 |
PJ-OQ | 966 | 900 | 600 | 600 | 500 | 150 |
PJ-OQ | 1077 | 1000 | 700 | 700 | 700 | 200 |
PJ-OQ | 1288 | 1200 | 800 | 800 | 1000 | 240 |
PJ-OQ | 1599 | 1500 | 900 | 900 | 1200 | 300 |
Iwọn otutu iṣẹ:150 ℃-1250 ℃; Isokan iwọn otutu:≤±5℃; Igbale Gbẹhin:4*10-1Pa / 6.7*10-3Pa; Iwọn igbega titẹ:≤0.67Pa/h; Epo quenching otutu:60-80 ℃, adijositabulu ati ibakan.
|
Akiyesi: Iwọn adani ati sipesifikesonu wa.